50H230 Non Grain Oriented Electrical steel
The cold-rolling process used to produce 50H230 Non Grain Oriented Electrical steel ensures that it has a uniform thickness and a smooth surface, which is important for maintaining consistent magnetic properties.

50H230 Electrical steel Specifications
| Thickness | Assumed Density |
Core Loss(W/Kg) | Core Loss(W/Lb) | Induction (800A/m) |
Lamination Factor (Minimum) |
Remark | ||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 50Hz | 60Hz | 50Hz | 60Hz | |||||||||
| mm | Kg/dm3 | 1.0T | 1.5T | 1.0T | 1.5T | 1.0T | 1.5T | 1.0T | 1.5T | |||
| 0.50 | 7.60 | 1.00 | 2.30 | 1.30 | 2.95 | 0.45 | 1.04 | 0.59 | 1.34 | 1.62 | 96.0 | - |
50H230 Electrical steel Typical Electrical and Magnetic Properties
| Assumed Density |
Resistivity | Core Loss | Induction T |
||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| W/Kg | W/LB | ||||||||||
| Kg/dm3 | Ohm*Meter (X10e-8) |
50Hz | 60Hz | 50Hz | 60Hz | ||||||
| 1.0T | 1.5T | 1.0T | 1.5T | 1.0T | 1.5T | 1.0T | 1.5T | 2,500A/m | 5,000A/m | ||
| 7.60 | 59 | 0.96 | 2.26 | 1.23 | 2.90 | 0.44 | 1.03 | 0.56 | 1.32 | 1.57 | 1.67 |
50H230 Electrical steel Typical Mechanical Properties and Lamination Factors
| Tensiile Strength | Yield Point | Elongation % |
Hardness Hv(1) |
Bending Test Value |
Lamination Factor % |
||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| N/mm2 | lb/in2(X10e3) | N/mm2 | lb/in2(X10e3) | ||||||||||
| L | C | L | C | L | C | L | C | L | C | L | C | ||
| 530 | 549 | 77 | 80 | 441 | 461 | 64 | 67 | 14 | 20 | 205 | 6 | 6 | 98.5 |